Surface integrity investigation of a Zr<SUB align="right">52.5Ti<SUB align="right">5Cu<SUB align="right">17.9Ni<SUB align="right">14.6Al<SUB align="right">10 metallic glass after grinding - CNRS - Centre national de la recherche scientifique Access content directly
Journal Articles International Journal of Machining and Machinability of Materials Year : 2020

Surface integrity investigation of a Zr52.5Ti5Cu17.9Ni14.6Al10 metallic glass after grinding

Bruno Lavisse
  • Function : Author
Nassim Mendil
  • Function : Author
Georges Kapelski
  • Function : Author
Xavier Cerutti
  • Function : Author
  • PersonId : 783074
  • IdRef : 190410183
Alexis Lenain
  • Function : Author
Sébastien Gravier
  • Function : Author
No file

Dates and versions

Identifiers

Cite

Bruno Lavisse, Nassim Mendil, Georges Kapelski, Xavier Cerutti, Alexis Lenain, et al.. Surface integrity investigation of a Zr52.5Ti5Cu17.9Ni14.6Al10 metallic glass after grinding. International Journal of Machining and Machinability of Materials, 2020, 22 (5), pp.430. ⟨10.1504/IJMMM.2020.109853⟩. ⟨hal-03048058⟩